Improvement and prevention plans for PCB soldering defects:

Data:

2023-12-08


Reduce the current density and perform regular maintenance or weak electrolysis treatment on the filter system.

Use solvent to clean the debris. If it is silicone oil, then you need to use a special cleaning solvent for cleaning.

Control the temperature during PCB soldering to 200-300°C and ensure sufficient preheating time.

Use flux correctly.

 

 